DSC/thermal analysis: melting and crystallisation behaviour

DSC run (Differential Scanning Calorimetry) for determination of crystal melting point Tpm and melting enthalpy delta H (further characteristics, e. g. crystallisation temperature Tc, depending on material, available on request) by means of two heating runs.

test method:Material analysis
Norms: DIN EN ISO 11357-3 (2018-07)
Needed sample size:Minimum 100 mg (min. 100 g for measurements on material to be ground)

Standardprüfungen

DSC heating up to 200°C (for PE, PP, etc.)
This method is common for all kinds of articles made out of PE and it's copolymers as well for PP (e.g. films, granules, moulded parts, etc.), other test parameters on request.


DSC heating up to 300°C (for laminated films, PA, PET, etc.)
This method is common for all kinds of articles made out raw materials which are more heat resistant (e.g. laminated films, PA, PET, EVOH etc.), other test parameters on request.