+49 441 94986-0

Information about tests

Moisture content/water content (residual moisture)

The choice of the appropriate method depends essentially on the expected moisture content. Higher water contents can be determined gravimetrically well with the drying oven technique. When lower water contents are expected, the water selective Karl Fischer titration should be chosen, as incorrect measurements, for example by other volatile matters can be excluded. The Karl Fischer method is, however, not intended for determination of higher water contents.

test method:Material analysis
Norms: DIN 51777 (2020-04)
DIN EN ISO 15512 (2019-09)
Needed sample size:At least 10 g of the material, if necessary hermetically packed, to avoid moisture content changes during transport.

Standardprüfungen

Moisture content of, liquid samples, e.g. solvents, printing inks, laquers
The test is carried out with the water-selective Karl Fischer method. In the case of liquid samples, e.g. Solvent, these could be analyzed directly. This method is particularly suitable for low absolute levels well below one percent down to a few ppm.
Norm: DIN 51777-1


Moisture content of plastics (e.g. granulates, plastic films, cold sealants)
The test is carried out with the water-selective Karl Fischer method. Solid samples, e.g. plastic resins or plastic films, are heated prior to the measurement in a furnace and the extracted gas phase is led for analysis in the Karl Fischer solution. This method is particularly suitable for low absolute levels well below one percent down to a few ppm, So for example, also of determining the residual moisture in thin coatings (e.g., dispersions) on moisture-free carrier films (e.g. of polyethylene).
Norm: DIN EN ISO 15512 B2


Moisture of paper/board
The test is performed by gravimetry according to the traditional oven drying method. This is not selective for water, other volatiles are also detected. The method is therefore only suitable for higher water contents and samples with a negligible amount of other volatiles besides water. The samples, as desired, are tested as received (without condioning) or after conditioning in a standard climate 23/50 or a climate according to your information. The moisture retention of the samples are usually in the lower percentage range.
Norm: DIN EN ISO 15512


Moisture content, substrate with coating
This method can be used, for example, to determine the moisture content of acrylate dispersions on polyethylene films.
Norm: DIN EN ISO 15512




back to overview Material analysis